The object print slowly, layer height be low.
Big Object settings
like object - speed 40-50 Layer height 0.1
So so object - speed 60- Layer height 0.2
Layer height decide the object to be fine, then speed.
流動性太好的線材, 拉絲也會很多
流動性太好的意思是易融
所以還沒到固定要印的位置
料就流出來了
如. 木頭紋的線材. 拉絲會很多
有色的線,愈是不透光噴嘴溫度要愈高。
[CR7] clean nozzleClean nozzle step by step by following youtube.Cr7清理噴頭
Because my nozzle alway inject too many PLA. So I google many websit, and decide to clean my …Read More
[3DP] Limit Switch Replace
The connection method follow the picture.
Red - Red
Green - Green
Red - Vcc
Black - Ground
Green - Signal
Reference:
- Mechanical E…Read More
[Cura] Information
firm the object stable
Support
Brim or raft
Platform Adhesion
CURA操作秘笈大公開
Line
Cura完整設定
…Read More
0 意見:
張貼留言